The temperature required for full annealing in hyper-eutectoid steel is
A:
30° C to 50° C above upper critical temperature
B:
30° C to 50° C below upper critical temperature
C:
30° C to 50° C above lower critical temperature
D:
30° C to 50° C below lower critical temperature
Answer:
C
No answer description is available.
Let's discuss.
Discuss About this Question.
Post
The alloy, mainly used for corrosion resistance in stainless steels is
A:
silicon
B:
manganese
C:
carbon
D:
chromium
Answer:
D
No answer description is available.
Let's discuss.
Discuss About this Question.
Post
A steel containing 16 to 18% chromium and about 0.12% carbon is called
A:
ferritic stainless steel
B:
austenitic stainless steel
C:
martensitic stainless steel
D:
nickel steel
Answer:
A
No answer description is available.
Let's discuss.
Discuss About this Question.
Post
In low carbon steels, __________ raises the yield point and improves the resistance to atmospheric corrosion.
A:
sulphur
B:
phosphorus
C:
manganese
D:
silicon
Answer:
B
No answer description is available.
Let's discuss.
Discuss About this Question.
Post
Shock resistance of steel is increased by adding
A:
nickel
B:
chromium
C:
nickel and chromium
D:
sulphur, lead and phosphorus
Answer:
C
No answer description is available.
Let's discuss.
Discuss About this Question.
Post
Ad Slot (Above Pagination)
‹ Prev
1
2
3
4
5
6
7
8
9
10
11
12
13
14
15
16
17
18
19
20
21
22
23
24
25
26
27
28
29
30
31
32
33
34
35
36
37
38
39
40
41
42
43
44
45
46
47
48
49
50
51
52
53
54
55
Next ›
Install ExamAdept
Fast access — add this app to your device.
Install
✕
To install on iPhone/iPad: tap Share →
Add to Home Screen
.
Quiz
Discuss About this Question.